Post by FredC on Nov 2nd, 2018 at 6:28pm
Thanks for the info. I had tried using molten lead setting the heat with a thermometer. Then coated the case necks with oil before dipping them in the molten lead. The lead coated the case necks sometimes and made a mess.
I assume the potassium salts cause no corrosion or embrittlement if you clean them quickly?